Magnesia Alumina Spinel Brick

  • Magnesia Alumina Spinel Brick

Product Description And Parameters

Composition:MgO + Al2O3/Fe2O3/ZrO2

Application:Cement and lime Kiln, or other industrial kilns.

Raw Material:DBM & Spinel

Refractoriness:≥1790℃

Capacity:500 tons per month

Magnesia spinel bricks are refractory products made of periclase and magnesia alumina spinel ,which can improve the heat stability of common magnesia brick.

Features
1.Excellent Heat Stability.
2.Better Anti-stripping performance than direct bonded magnesia chrome brick.
3.Abrasion Resistant.
4.High Refractoriness Under Load.

Application
It’s mainly used for burning zone and transition zone of cement kiln, also some other industrial furnaces.

Product

Magnesia Alumina Spinel Bricks

Magnesia AluminaSpinel Zirconium Bricks

Magnesia Spinel Bricks

Magnesia Alumina Zirconium Bricks

Model

MLJ-85A

MLJ-93A

MLJ-95A

MLJ-85B

MLJ-93B

MLJ-95B

MLJZ-93A

MLJZ-93B

MLJZ-R63A

MLJZ-R63B

MZ-96A

MZ-94B

MgO% ≤

85

88

93

82

85

90

92

88

85

80

92

88

Al2O3 ≤

9

5

3

9

5

3

5

5

3

3

5

5

Fe2O3≤

0.7

0.7

0.7

0.8

0.8

0.8

0.7

0.8

7.5

7.5

0.8

0.9

SiO2 ≤

0.6

0.8

0.7

2.5

2

2.5

1

2.5

0.9

2.0

1

2.5

ZiO2 ≤

 

 

 

 

 

 

1-3

1-3

 

 

1-3

1-3

Apparent Porosity ≤

16-18

16-18

16-18

17-18

17-18

17-18

17-18

17-18

16-17

16-17

17-19

17-19

Bulk Density ≤

2.85

2.85-3.0

2.85

2.8

2.85

2.82

2.85

2.8

30.

2.9

2.9

2.8

Cold Crushing Strength ≤

45

45

45

40

40

40

50

50

50

45

50

45

0.2.Mpa Refractoriness Under Load(℃) ≤

1700

1700

1700

1700

1700

1700

1700

1660

1660

1630

1700

1650

Thermal Expansion1400℃

 

 

 

 

 

 

 

 

 

 

1.6

1.6

Thermal Shock Resistance

1100℃ water cooling, times

12

12

12

10

10

10

12

10

10

8

8

6

950℃water cooling, times

100

100

100

80

80

80

100

80

100

80

30

25

Heat Conductivity

2.8

2.9

3.0

2.8

2.9

3.0

3.0

2.9

2.5

2.5

4.5

4.4